Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 93000 cP @Temperature 25.0 °C |
93000 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Cast 3109 Low Cost Epoxy Casting System TRA-CAST 3109 is a versatile epoxy casting system developed for solvent-free production casting, potting, encapsulating, and coating applications where low cost, easy handling and flowability, and e.. |