Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 9.8 cP @Temperature 20.0 °C |
9.8 cP @Temperature 68.0 °F |
|
LG Chemical 2-EH 2-Ethyl Hexanol Applications: Plasticizers, stabilizers, solvents, acrylatesCAS: 104-76-7Information provided by LG Chemical |