Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 890 cP @Temperature 25.0 °C |
890 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Cast F311 Optically Transparent Semi-Flexible Casting System TRA-CAST F311 is a clear, low viscosity epoxy formulation developed for molding, embedding, casting and potting applications where clarity, toughness, long pot-life and superior impact properties ar.. |
|||
Viscosity | 890 cP | 890 cP | 25% Toluene solution; ASTM D2994 |
Dynasol Solprene® 4302 Thermoplastic Rubber (SBS) Solprene 4302 is a linear block copolymer of styrene and butadiene, having 31% styrene content, most of it forming a polystyrene block, which gives the polymer a thermoplastic behavior. It has a non.. |