Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 870 cP @Temperature 25.0 °C |
870 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Cast 3011 Semi-Flexible Clear Epoxy Casting Compound TRA-CAST 3011 is a clear, low viscosity epoxy casting compound recommended for industrial embedding and casting applications where its combination of superior properties, good clarity, long pot life.. |