Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 8600 cP @Shear Rate 10994 1/s, Temperature 210 °C |
8600 cP @Shear Rate 10994 1/s, Temperature 410 °F |
ASTM D3835 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7375-1000 TPE Product Description: StarFlex P 7375-1000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades avai.. |
|||
Viscosity | 8600 cP @Shear Rate 10994 1/s, Temperature 210 °C |
8600 cP @Shear Rate 10994 1/s, Temperature 410 °F |
ASTM D3835 |
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 40-LR-1 TPE Product Description: StarTUFF TF 40-LR-1 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M.. |
|||
Viscosity | 8600 cP @Shear Rate 10994 1/s, Temperature 210 °C |
8600 cP @Shear Rate 10994 1/s, Temperature 410 °F |
ASTM D3835 |
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 75-LR-9 TPE Product Description: StarTUFF TF 75-LR-9 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M.. |
|||
Viscosity | 8600 cP @Shear Rate 10994 1/s, Temperature 210 °C |
8600 cP @Shear Rate 10994 1/s, Temperature 410 °F |
ASTM D3835 |
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 40-LR-9 TPE Product Description: StarTUFF TF 40-LR-9 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M.. |
|||
Viscosity | 8600 - 9600 cP @Temperature 35.0 °C |
8600 - 9600 cP @Temperature 95.0 °F |
|
C.O.I.M. DIEXTER® G196 Polyol Polyester Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt.. |