Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 860 - 2500 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
860 - 2500 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2061027P15 High Brightness Phosphor Ink (Blue) This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera.. |
|||
Viscosity | 860 - 2500 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
860 - 2500 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2070126D4 High Brightness Phosphor Ink (Orange) This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera.. |
|||
Viscosity | 860 - 2500 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
860 - 2500 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2070126P5 High Brightness Phosphor Ink (White) This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera.. |
|||
Viscosity | 860 - 2500 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
860 - 2500 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2080211P2 High Brightness Phosphor Ink (Blue/Green & Blue) This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera.. |
|||
Viscosity | 860 - 2500 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
860 - 2500 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2101125P4 High Brightness Phosphor Ink This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera.. |