Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 175000 - 850000 cP @Temperature 400 - 420 °C |
175000 - 850000 cP @Temperature 752 - 788 °F |
Average value: 513000 cP Grade Count:11 |
Overview of materials for Polyetheretherketone, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Viscosity | 350000 - 850000 cP @Temperature 400 - 400 °C |
350000 - 850000 cP @Temperature 752 - 752 °F |
Average value: 445000 cP Grade Count:3 |
Overview of materials for Polyetheretherketone, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum.. |
|||
Viscosity | 350000 - 850000 cP @Shear Rate 1000 - 1000 1/s |
350000 - 850000 cP @Shear Rate 1000 - 1000 1/s |
Average value: 445000 cP Grade Count:3 |
Overview of materials for Polyetheretherketone, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum.. |