Physical Properties Metric English Comments
Viscosity 7300 - 8300 cP

@Temperature 35.0 °C
7300 - 8300 cP

@Temperature 95.0 °F
C.O.I.M. DIEXTER® G170 Polyol Polyester
Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt..
Viscosity 7300 - 8300 cP

@Temperature 35.0 °C
7300 - 8300 cP

@Temperature 95.0 °F
C.O.I.M. DIEXTER® G172 Polyol Polyester
Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt..