Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 825 cP @Temperature 25.0 °C |
825 cP @Temperature 77.0 °F |
|
Struktol STRUKSILON 8104 Silicone Stabilizer for PU Foam STRUKSILON 8104 was developed as universal silicone stabilizer of medium potency for the production of conventional flexible polyurethane slabstock foam based on polyether polyols.Applications: STRU.. |