Physical Properties Metric English Comments
Viscosity 7700 cP

@Shear Rate 10994 1/s,
Temperature 210 °C
7700 cP

@Shear Rate 10994 1/s,
Temperature 410 °F
ASTM D3835
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7350-1000 TPE
Product Description: StarFlex P 7350-1000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades avai..
Viscosity 7700 cP

@Shear Rate 10994 1/s,
Temperature 210 °C
7700 cP

@Shear Rate 10994 1/s,
Temperature 410 °F
ASTM D3835
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7360-1000 TPE
Product Description: StarFlex P 7360-1000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades avai..
Viscosity 7700 cP

@Shear Rate 10994 1/s,
Temperature 210 °C
7700 cP

@Shear Rate 10994 1/s,
Temperature 410 °F
ASTM D3835
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7360-9000 TPE
Product Description: StarFlex P 7360-9000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelGood WeatherabilityFDA and medical grades availableProcessing Method..