Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 768 cP | 768 cP | Toluene solution, 25%; NM 300-11 |
Dynasol Solprene® 4580X TPE Multiblock Solprene 4580X is a linear multiblock copolymer of styrene and butadiene with high vinyl (>25%), having 45% of styrene content, most of this one appears like block polystyrene, which gives the polym.. |