Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 757 cP @Temperature 23.0 °C |
757 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® AP-100 All-Purpose Adhesion Promoter Preliminary Product Information SheetMaterial Description: AP-100 is an all-purpose adhesion promoter. It can be used on glasses, metals, ceramics and most plastics found in electronic assembly and.. |