Polymer Property : Viscosity = 7425 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 7425 cP
7425 cP
Valley Adhesives EM-210 Low Temperature Application Glue Stick
Valley Adhesives EM-210 Low Temperature Application Glue StickMedium bonding range; bonds P.O.P. displays, paper, corrugated boxes, fabrics, furniture, upholstery, and other light weight heat sensit..