Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 740000 cP | 740000 cP | B |
Shin-Etsu Silicones LIMSâ„¢ KE1950-60A/B Elastomer KE-1950-60 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy .. |
|||
Viscosity | 740000 cP @Shear Rate 300 1/s, Temperature 190 °C |
740000 cP @Shear Rate 300 1/s, Temperature 374 °F |
ASTM D3835 |
Advanced Polymer Alloys Alcryn® 1070 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |