Polymer Property : Viscosity = 710 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 710 - 2150 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
710 - 2150 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Gwent Electronic Materials C2061027P13 High Brightness Phosphor Ink (Blue/Green)
This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera..