Polymer Property : Viscosity = 6300 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 6300 - 7700 cP
6300 - 7700 cP
ND Industries 567 Shaft & Bearing Retainer Retaining Compound
High temperature retainer for engine cylinder liners and heat exchanger tubes
Viscosity 6300 - 10000 cP

@Temperature 150 °C
6300 - 10000 cP

@Temperature 302 °F
542-111
Westlake Epolene® C-16P Coating Grade - Branched Medium Molecular Weight Polyethylene Polymer
Description: Epolene C-16P is a branched low density polyethylene powder modified with maleic anhydride. It is useful as a base polymer for adhesives and coatings, color concentrate dispersions, and..
Viscosity 6300 cP

@Temperature -20.0 °C
6300 cP

@Temperature -4.00 °F
Cold Cranking
ConocoPhillips Conoco® El Mar® 15W-40 Mid Ash Heavy Duty
Conoco® El Mar Mid Ash Heavy Duty is a high-quality, mid-ash, dispersant-detergent gas engine oil designed for use in naturally aspirated and moderately to highly turbocharged 4-stroke cycle natura..
Viscosity 6300 cP

@Temperature -20.0 °C
6300 cP

@Temperature -4.00 °F
Cold Cranking
ConocoPhillips Conoco® El Mar® Ashless Heavy Duty Oil, SAE Viscosity Grade 15W-40
Conoco® El Mar Ashless Heavy Duty is a high-quality, ashless, dispersant-detergent gas engine oil designed for use in naturally aspirated and moderately turbocharged 2-stroke cycle natural gas engi..