Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 60396 cP | 60396 cP | Mixed (cp #52, 2.5 rpm) |
Tra-Con Tra-Bond 970-1N1 General Purpose Epoxy Adhesive TRA-BOND 970-1N1 is a general purpose epoxy that exhibits sag resistance and excellent bond strength to a wide variety of substrates. Information provided by Tra-Con Inc. |