Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 5900 cP @Shear Rate 11200 1/s, Temperature 200 °C |
5900 cP @Shear Rate 11200 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne Versalloy™ XL 9055X-9 Thermoplastic Elastomer (TPE) Versalloy™ XL 9055X-9 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Overmold Adhesion to Polypro.. |
|||
Viscosity | 5900 cP | 5900 cP | 12% Solid, 1.5% NaCl |
Solvay MACKADET® EQ-178 Surfactant Product Description: Mackadet EQ-178 is a mild, concentrated blend of surfactants for use as a base for high foam personal care products. This blend is free of alcohol, diethanolamides, lauryl sulfa.. |
|||
Viscosity | 5900 cP @Temperature 25.0 °C |
5900 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond 526M02 High Tg Fiber Optic Adhesive TRA-BOND 526M02 is a two-part, low viscosity epoxy system that was developed specifically for fiber optic applications. This material is recommended for bonding fiber optic bundles, potting glass fi.. |
|||
Viscosity | 5900 cP | 5900 cP | |
Dow Corning JCR 6101 One-part, translucent, medium modulus LED encapsulant with very long working time.Information provided by Dow Corning |