Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 57500 cP | 57500 cP | Mixed (cp #52, 5 rpm) |
Tra-Con Tra-Duct 916H03 Room Temperature Cure High Conductivity Silver Epoxy Adhesive TRA-DUCT 916H03 is recommended for electronic bonding and sealing applications that require the combination of high conductivity coupled with good mechanical properties. This two part smooth paste s.. |