POLYMER SEARCH
Polymer Property : Viscosity = 55 cP
Polymer Property :
Viscosity =
55 cP
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Viscosity
20
-
55
cP
20
-
55
cP
Beijing Ranger Chem B-63 Liquid Epoxy Resin
Information provided by Beijing Ranger Chemical Co.