Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 53 cP @Temperature 25.0 °C |
53 cP @Temperature 77.0 °F |
Solution Viscosity in 5 wt.% Toluene; UBE Method |
UBE UBEPOL BR150B Non-Oil Extended Synthetic Rubber (Raw Polymer) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Microstructure: cis: 97trans: 2vinyl: 1Information provided by UBE. |
|||
Viscosity | 53 - 63 cP | 53 - 63 cP | |
Solvay RHODASURF® BC-610 Surfactant Description: Iso-tridecyl alcohol ethoxylate. HLB = 11.4. Low foaming wetting agents and emulsifiers liquid formulations.Chemical Name: NONIONIC EMULSIFIERCAS: 78330-21-9Available in: Asia Pacific, .. |