Physical Properties Metric English Comments
Viscosity 520 - 700 cP

@Temperature 25.0 °C
520 - 700 cP

@Temperature 77.0 °F
ACC EP Primer 28 EPI Engineered Polymers Aromatic polyisocyanate Prepolymer
EP Primer 28 is a polyisocyanate prepolymer based on diphenylmethane diisocyanate (MDI). As corrosion-resistant primers, coatings based on EP Primer 28 polyisocyanate can be formulated to contain z..
Viscosity 520 - 680 cP

@Temperature 25.0 °C
520 - 680 cP

@Temperature 77.0 °F
BorsodChem ONGRONAT CR-30-60 MDI Isocyanate
Polymethylene-polyphenyl-isocyanate, 4,4-diphenyl-methane-diisocyanate (MDI) and mixture of its higher functionality, multi-ring oligomers.Field of application: With suitable polyols it can be used ..