Physical Properties Metric English Comments
Viscosity 5001 cP
5001 cP
Valley Adhesives EM-105 High Performance Application Glue Stick
Valley Adhesives EM-105 High Performance Application Glue StickHigh peel, shear strength, and heat resistance; Good wetting and heat resistance for potting; Excellent adhesion to wood, plastics, pol..