Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 5.60e+14 cP @Temperature 1100 °C |
5.60e+14 cP @Temperature 2010 °F |
|
Momentive Performance Materials Type 219 Fused Quartz Tubing Known as "Ozone-Free" or "Germicidal" quartz tubing. Transmits UV-A and UV-B while blocking the deep, high energy wavelengths that cause ozone generation and pose the greatest exposure risks. Tran.. |