Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 480000 cP | 480000 cP | A |
Shin-Etsu Silicones LIMSâ„¢ KE1950-40A/B Elastomer KE-1950-40 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy .. |
|||
Viscosity | 480000 cP | 480000 cP | B |
Shin-Etsu Silicones LIMSâ„¢ KE1950-40A/B Elastomer KE-1950-40 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy .. |
|||
Viscosity | 480000 cP @Shear Rate 1000 1/s, Temperature 260 °C |
480000 cP @Shear Rate 1000 1/s, Temperature 500 °F |
melt viscosity; b.o. ISO 11443-A |
Covestro Bayblend® FR3050 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |