Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 473000 cP @Frequency 1000 Hz, Temperature 177 °C |
473000 cP @Frequency 1000 Hz, Temperature 351 °F |
Melt Viscosity; ASTM D3835 |
Teknor Apex Fireguard® 910L16-C13-NL Polyvinyl Chloride, Flexible Notes: RoHS Compliant Features: Flame Retardant; Low Smoke Emission Uses: Plenum Cable Jacketing Wire Types: CL2P; CL3P; CMP; FPLP; MPP; OFNP Agency Ratings: NEC Article 725; NEC Article 760; NEC Ar.. |
|||
Viscosity | 473000 - 473000 cP @Temperature 177 - 177 °C |
473000 - 473000 cP @Temperature 351 - 351 °F |
Average value: 473000 cP Grade Count:1 |
Overview of materials for PVC, Wire and Cable Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Wire and Cable Grade". Each property range of values reported is minimum and maximum values of appr.. |
|||
Viscosity | 473000 - 473000 cP @Frequency 1000 - 1000 Hz |
473000 - 473000 cP @Frequency 1000 - 1000 Hz |
Average value: 473000 cP Grade Count:1 |
Overview of materials for PVC, Wire and Cable Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Wire and Cable Grade". Each property range of values reported is minimum and maximum values of appr.. |