Physical Properties Metric English Comments
Viscosity 24000 - 46000 cP

@Temperature 23.0 °C
24000 - 46000 cP

@Temperature 73.4 °F
5 rpm
Epoxy Technology EPO-TEK® EV2002 Silver-filled, electrically conductive, flexible epoxy
Material Description: Silver-filled, electrically conductive, flexible epoxyInformation Provided by Epoxy Technology