Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 455400 cP @Shear Rate 500 1/s, Temperature 260 °C |
455400 cP @Shear Rate 500 1/s, Temperature 500 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS 30G30HSL BK038A Nylon 610 30% Glass Reinforced Renewably Sourced Polyamide 610 Developed for Extrusion Information provided by DuPont Performance Polymers |