Polymer Property : Viscosity = 42000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 24000 - 42000 cP

@Temperature 23.0 °C
24000 - 42000 cP

@Temperature 73.4 °F
2.5 rpm
Epoxy Technology EPO-TEK® OD2002 High Temperature Epoxy
Material Description: High Tg version of EPO-TEK®353ND with low modulus and good toughness. Replacement for EPO-TEK® 364. Complies with USP Class VI biocompatibility standards.Information Provid..