Physical Properties Metric English Comments
Viscosity 4.4 cP

@Temperature 25.0 °C
4.4 cP

@Temperature 77.0 °F
LyondellBasell DPNP Dipropylene glycol normal propyl ether
Information provided by Lyondell.