Physical Properties Metric English Comments
Viscosity 34000 - 38000 cP

@Shear Rate 50.0 1/s,
Temperature 25.0 °C
34000 - 38000 cP

@Shear Rate 50.0 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Gwent Electronic Materials C2070117D2 Gold Ink
Gold Ink C2070117D2 is a fritted system that has been designed as a screen printing ink for uses on Alumina. It is also suitable for firing onto other high temperature substrates. This ink has bee..