Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 3800 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
3800 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials D2020823D2 Polymer Dielectric This material is a blue colored screen printable polymer Dielectric, suitable for defining electrode areas and forms a protective layer over the electrode tracking during immersion of the electrode... |