Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 38 - 47 cP @Temperature 20.0 °C |
38 - 47 cP @Temperature 68.0 °F |
|
Oceanchem Group Tris (chloroethyl) Phosphate (TCEP) Molecular Formula: C6H12O4Cl3PCas No.: 29716-44-7Property: It is colorless or light yellow oily transparent liquid with slight cream odor. Soluble in common organic solvents, insoluble in aliphatic.. |
|||
Viscosity | 38 cP | 38 cP | Viscosity of Solution; 5% Styrene |
KKPC KOSYN KBR 720 Polybutadiene Rubber (Low cis BR) Polybutadiene Rubber (Low cis BR)Characteristics: Low cis BR is different in cis content according to the production process and the catalyst. KKPC's low cis LBR has 35% cis content. LBR has hi.. |
|||
Viscosity | 38 - 45 cP | 38 - 45 cP | |
Dow Corning XIAMETER® PMCPPMX-0930 Silanol Fluid Is chemically equivalent to DOW CORNING® 4-2737 FLUID. A polydimethylsiloxane polymer with terminated, curable silanol functionality.Information provided by Dow Corning |