Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 365 cP | 365 cP | Fed Std Method 4287 |
Humiseal 1B73LSE Acrylic Conformal Coating Humiseal 1B73LSE Acrylic Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesSelective chemical resistanceExcellent repairabilityUL Approval PendingMIL-I-46058C Approval Pendin.. |