Viscosity 360000 - 360000 cP

@Temperature 250 - 250 °C
360000 - 360000 cP

@Temperature 482 - 482 °F
Average value: 221000 cP Grade Count:1
Overview of materials for Nylon 610
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..