Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 360 cP | 360 cP | |
Von Roll Isola IMI Varnish 3255 Solventless Polyester Varnish for Electrical Insulation Data provided by Von Roll Isola USA.IMI solventless resins provide relatively void-free insulation for greater protection against severe environments and corona breakdown. Flash Point: >93°C. Usa.. |