Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Viscosity = 345000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 110000 - 345000 cP
110000 - 345000 cP
Thixotropic
Loctite® 5205 Flexible Cure Flange Sealant
Anaerobic GasketingLoctite® 5205 Flexible Cure Flange SealantFast curing and flexible, good sealing properties against oil and water/glycol particularly at high temperatures. High viscosity. Recom..
Viscosity 110000 - 345000 cP
110000 - 345000 cP
Thixotropic
Loctite® 5206 Flexible Cure Flange Sealant
Anaerobic GasketingLoctite® 5206 Flexible Cure Flange SealantSlow curing allows for micro-movement during assembly operations. Good sealing properties against oil and water/glycol. High viscosity...
Copyright © lookpolymers.com All Rights Reserved