Viscosity 310000 cP
310000 cP
Melt Viscosity, 200°C, 1000 sec-1; ASTM D3825
SABIC Innovative Plastics Cycolac® FR23 ABS
Flame retardant ABS (non-PBBE additives). Good properties/toughness. Excellent moldability. UL94 V-0 rated.
Viscosity 310000 cP
310000 cP
Melt Viscosity, 200°C, 1000 sec-1; ASTM D3825
SABIC Innovative Plastics Cycolac® FR23 ABS (Asia Pacific)
Flame retardant ABS (non-PBBE additives). Good properties/toughness. Excellent moldability. UL94 V-0 rated.
Viscosity 310000 cP
310000 cP
Melt Viscosity, 260°C, 1500 sec-1; ISO 11443
SABIC Innovative Plastics Valox® 357X PBT (Europe-Africa-Middle East)
VALOX 357X is an impact modified, flame retarted PBT+PC blend. Applications like bobbins, switches and enclosures.
Viscosity 310000 cP

@Shear Rate 206 1/s,
Temperature 200 °C
310000 cP

@Shear Rate 206 1/s,
Temperature 392 °F
ASTM D3835
Teknor Apex Sarlink® 3180 Thermoplastic Elastomer
A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3180 can be processed by blow molding injection molding or ex..