Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 3050 cP @Temperature 25.0 °C |
3050 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond 5126 Medium Viscosity Aerospace-Grade Epoxy Adhesive TRA-BOND 5126 AEROSPACE-GRADE EPOXY ADHESIVE is a two-part, clear (amber), medium viscosity, aerospace-grade epoxy adhesive system recommended for bonding a wide variety of materials for structural .. |