Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 28500 cP @Temperature 25.0 °C |
28500 cP @Temperature 77.0 °F |
Mixed (rv #6, 10 rpm) |
Tra-Con Tra-Bond FDA25 Food and Drug Application Epoxy Adhesive TRA-BOND FDA-25 is a medium viscosity epoxy resin system specifically developed for bonding and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and Drug Admi.. |