Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 2750 cP | 2750 cP | |
Master Bond Mastersil 153 Two Component, High Temperature Resistance Silicone Adhesive Master Bond MasterSil 153 is a two component, paste silicone compound for high performance bonding and sealing. MasterSil 153 is an addition cured system and does not require exposure to air for com.. |