Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 130 - 2580 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
130 - 2580 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2011004P5 Platinum Ink Platinum Ink is designed for oxygen sensor applications. This is a pure platinum ink with no inorganic additions to give maximum response to oxygen. It is suitable for firing on to other high tempe.. |