Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 253100 cP @Shear Rate 500 1/s, Temperature 260 °C |
253100 cP @Shear Rate 500 1/s, Temperature 500 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® HR5330HFS NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate with Improved Processing Crastin HR5330HFS is a 30% glass fiber reinforced moderately toughened hydrolysis resistant polybutylene terephthalate for in.. |