Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 16000 - 24000 cP | 16000 - 24000 cP | 30% solid in Anone |
Taiwan Sheen Soon Sheenthane® A7711 TPU for Ink Thermoplastic polyurethane elastomer for ink. Hydrolysis resistance gradeAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen.. |
|||
Viscosity | 19000 - 24000 cP | 19000 - 24000 cP | |
Beijing Ranger Chem SM828S Liquid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |