Physical Properties Metric English Comments
Viscosity 22500 cP
22500 cP
Mixed 1:1; TM R050-12
Resinlab® EP1215 Clear Unfilled Epoxy Structural Adhesive
Resinlab™ EP1215 Clear is a two part unfilled epoxy structural adhesive designed for bonding applications requiring high strength and good impact resistance. It cures completely at room temperature..
Viscosity 22500 cP
22500 cP
Part B at 20 RPM
Loctite® 3273 Acrylic Bonding Adhesive
Acrylic Bonding AdhesivesLoctite® Acrylic Adhesives were developed for bonding applications that require tensile, shear and peel strength combined with maximum impact, stress and shock resistance. ..
Viscosity 22500 cP

@Temperature 25.0 °C
22500 cP

@Temperature 77.0 °F
Mixed (sp #6, 10 rpm)
Tra-Con Tra-Cast 3107 Low Shrinkage Epoxy Casting System
TRA-CAST 3107 is a versatile epoxy casting system developed for high performance production potting, encapsulating, casting and tooling applications where low shrinkage, easy handling and flowabilit..