Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 22 cP | 22 cP | D=30/s; DIN 54 453 |
3M Dyneon™ TF 5060 PTFE Dispersion
(discontinued **) Typically used for coating of glass fiber fabricsInformation provided by the Dyneon division of 3M. |
|||
Viscosity | 22 cP | 22 cP | D=30/s; DIN 54 453 |
3M Dyneon™ TF 5032 PTFE Dispersion
(discontinued **) Used for impregnation.Dyneon PTFE dispersions are aqueous dispersions developed for use in metal coating formulations and for application of impregnation and fabric coating applications. A range of .. |
|||
Viscosity | 22 cP | 22 cP | |
Asahi Glass Fluon® AD639 PTFE Aqueous Dispersion Fluon®PTFE aqueous dispersions are useful for glass cloth coating, metal coating, binder, additive in resin, feedstock of heat resistive paint ,etc.Information provided by Asahi Glass Company, Inc... |