Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 215000 cP | 215000 cP | Melt Viscosity, 260°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Valox® 325 PBT (Europe-Africa-Middle East) VALOX 325 is a general purpose, unreinforced PBT injection moulding resin. Applications: sprinklers and nozzles, pumps, doorhandles, tank covers, pens and pencils. |
|||
Viscosity | 215000 cP | 215000 cP | Melt Viscosity, 260°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Valox® VX5022 PBT (Europe-Africa-Middle East) VALOX VX5022 is a 20% glass fibre reinforced PBT+PC blend with low warpage characteristics. This grade is 5021 with reduced warpage. |
|||
Viscosity | 215000 cP | 215000 cP | Melt Viscosity, 260°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Xenoy® X5100 PC+PBT (Europe-Africa-Middle East) XENOY X5100 is a semi-crystalline, impact modified PC-PBT blend with excellent flow. (PC+PBT-I). |
|||
Viscosity | 215000 cP @Temperature 250 °C |
215000 cP @Temperature 482 °F |
DAM; @ 1000 sec-1; ISO 11443 |
DuPont Performance Polymers Zytel® RS LC1201 BK040A Nylon 1010
(Unverified Data**) Toughened Renewably Sourced Medium Viscosity Polyamide 1010 Developed for Extrusion Zytel RS LC1201 BK040A is a renewably sourced polyamide 1010 resin containing a minimum of 85% renewably sourced i.. |