Physical Properties Metric English Comments
Viscosity 2150 cP
2150 cP
ACC EP MAP-Z 10 EPI Engineered Polymers Aliphatic Polymer
EP MAP Z, “Powered by Reactamine® Technology”, are zinc modified aliphatic prepolymers with monomer-extracted levels of a maximum of 0.2%. The polymers are made from HDI. Three products are avail..