Polymer Property : Viscosity = 2.27 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 0.680 - 2.27 cP
0.680 - 2.27 cP
Average value: 1.48 cP Grade Count:11
Overview of materials for PVC, Molded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb..