Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 190400 cP @Shear Rate 3000 1/s, Temperature 191 °C |
190400 cP @Shear Rate 3000 1/s, Temperature 375 °F |
Melt Viscosity |
Spartech Royalite R59M Hi-Impact ABS/PVC Resin Data provided by the manufacturer. A unique ABS/PVC resin that meets the flammability standards of many industries and is a cost-effective alternative to standard fire-rated ABS. High rigidity in t.. |